RSS 3

RSS 3

Contact
Product Description .
  • Slight resinous matter (rust) and slight amounts of dry mould on wrapper, bale surfaces and interior sheet, found at time of delivery will not be objected to.
    Should “Rust” or “Dry mould” in an appreciable extent appear on more than 10% of the bales sampled, it shall constitute grounds for objection.
    Slight blemishes in color, small bubbles and small specks of bark permissible to the extent shown in the sample.
    Oxidized spots or streaks, weak, heated, under-cured, over-smoked, opaque and burnt sheets are not permissible.
    The rubber must be dry, strong and free of blemishes, blisters, sand, dirty packing and all other foreign matter other than specifed above as permissible.